Aircraft Cleaning and Corrosion Control | FAA A&P Study Guide
Prepare Smart, Study Strong, Pass with Confidence

Aircraft cleaning procedures involve much more than a cosmetic task. Dirt, oil, exhaust residue, salt, moisture, battery electrolyte, and other contaminants can hide defects, damage protective finishes, interfere with electrical systems, and accelerate corrosion.
For students preparing for the FAA General Knowledge test, cleaning and corrosion control include understanding why aircraft are cleaned, how corrosion develops, how different metals react, where corrosion is most likely to occur, and how technicians inspect, remove, treat, and prevent corrosion. Study aircraft cleaning and corrosion control, including corrosion types, inspection, removal, prevention, avionics corrosion, AC 43-4B, and AC 43-206.
The FAA Aviation Maintenance Technician Handbook—General provides the foundation for this subject. The FAA also publishes two important advisory circulars:
- FAA AC 43-4B, Corrosion Control for Aircraft, which addresses corrosion affecting aircraft structures and engine materials.
- FAA AC 43-206 Change 1, Inspection, Prevention, Control, and Repair of Corrosion on Avionics Equipment, which addresses electrical and avionics systems and was updated in 2024.
These advisory circulars provide acceptable methods, techniques, and practices, but they do not replace current aircraft manufacturer instructions. When a manufacturer provides a corrosion-control program, inspection schedule, cleaning process, or repair procedure, technicians must follow the applicable manufacturer information.
At Volarprep.com, FAA A&P students can reinforce cleaning and corrosion-control knowledge using FAA-style practice questions supported by detailed explanations and applicable FAA references.
Why Aircraft Cleaning Is Important
A clean aircraft is easier to inspect. Dirt, grease, oil, and exhaust deposits may cover cracks, loose fasteners, fluid leaks, damaged coatings, and early evidence of corrosion.
Cleaning helps technicians:
- Locate fluid leaks
- Inspect aircraft structure
- Identify damaged paint and protective coatings
- Remove corrosive deposits
- Keep drain passages open
- Reduce fire hazards
- Protect electrical and avionics equipment
- Maintain aircraft appearance
- Prepare surfaces for inspection or refinishing
Cleaning must be performed correctly. Using an improper chemical, abrasive, brush, pressure, or cleaning method can damage aircraft materials, windows, seals, wiring, finishes, and components.
Technicians must identify the material and contaminant before selecting a cleaning process.
What Is Aircraft Corrosion?

Corrosion is the deterioration of metal caused by chemical or electrochemical interaction with its environment. It gradually converts metal into compounds such as oxides, hydroxides, or sulfates.
Corrosion is not the same as erosion. Corrosion involves a chemical or electrochemical reaction, while erosion is the mechanical wearing away of material.
The four conditions needed to establish an electrochemical corrosion cell are:
- An anode—a metal area that will corrode
- A cathode—a conductive material that is less likely to corrode
- An electrolyte—a conductive liquid, such as contaminated water
- An electrical path between the anode and cathode
Removing any one of these conditions can interrupt the corrosion process. Paint, sealant, plating, conversion coatings, and corrosion-preventive compounds help isolate aircraft metal from the surrounding environment.
Factors That Affect Corrosion
The rate, severity and types of aircraft corrosion depend on several factors:
- Type and condition of the metal
- Heat treatment and grain direction
- Contact between dissimilar metals
- Temperature
- Humidity
- Saltwater or salt-laden air
- Industrial pollution
- Battery electrolyte
- Availability of oxygen
- Mechanical stress
- Biological contamination
- Time exposed to the environment
- Condition of protective coatings
- Drainage and moisture retention
Aircraft operated near oceans, in humid climates, around industrial pollution, or in agricultural operations may require more aggressive aircraft corrosion inspection and prevention.
However, aircraft in dry climates are not immune. Moisture can collect inside enclosed structures, beneath insulation, around fasteners, or in poorly drained areas.
Direct Chemical and Electrochemical Attack
Aircraft corrosion can develop through direct chemical attack or electrochemical attack.
Direct chemical attack occurs when a metal reacts directly with a corrosive substance. Battery acid, spilled chemicals, cleaning compounds, and trapped fumes can attack aircraft materials.
Electrochemical attack occurs when an anode, cathode, electrolyte, and electrical path form a corrosion cell. One area of metal deteriorates while the chemical reaction is supported by another area.
Understanding these processes helps A&P students recognize why moisture, contaminants, and dissimilar-metal contact must be controlled.
Surface Corrosion
Surface corrosion is a relatively uniform attack across a metal surface. It may appear as roughness, etching, discoloration, or powdery corrosion products.
On aluminum, surface corrosion often appears as a white or gray powder. On ferrous metals, it normally produces reddish-brown rust.
Surface corrosion may appear minor, but the technician must determine whether damage extends below the visible surface.
Pitting Corrosion
Pitting corrosion produces small cavities or holes in the metal surface. It can be difficult to evaluate because a small surface opening may conceal deeper damage.
Pitting is common on metals that depend on a thin protective oxide film. Once the film breaks down, concentrated corrosion can continue beneath the surface.
The depth and location of a pit may be more important than its surface diameter. Corrosion removal and remaining material thickness must be evaluated using approved data.
Galvanic Corrosion

Galvanic corrosion occurs when dissimilar metals are electrically connected in the presence of an electrolyte.
One metal acts as the anode and corrodes more rapidly, while the other acts as the cathode. The difference between the metals’ positions in the galvanic series influences the severity of the reaction.
For example, magnesium structure in contact with steel hardware can experience severe galvanic attack when moisture bridges the two materials.
Galvanic corrosion prevention may involve:
- Selecting compatible materials
- Applying protective finishes
- Using sealant or insulating material
- Preventing moisture entry
- Maintaining drainage
- Following the manufacturer’s fastener and installation specifications
Technicians must never substitute hardware or materials without confirming compatibility and approval.
Concentration-Cell Corrosion

Concentration-cell corrosion develops when different areas of a metal surface are exposed to varying concentrations of oxygen or an electrolyte.
It frequently occurs in:
- Crevices
- Lap joints
- Beneath gaskets
- Beneath deposits
- Around fasteners
- Under loose paint
- Areas where water becomes trapped
The low-oxygen area commonly becomes anodic and corrodes.
Keeping joints properly sealed, drain passages open, and surfaces free from deposits helps prevent this form of corrosion.
Intergranular Corrosion
Intergranular corrosion attacks the grain boundaries within a metal alloy. Improper heat treatment or alloy conditions may make the material at the grain boundaries more chemically active than the grains themselves.
Because the attack can progress beneath the surface, intergranular corrosion may exist before significant exterior damage becomes visible.
When corrosion products force the metal grains apart and lift the surface into layers, the damage is known as exfoliation corrosion.
Intergranular and exfoliation corrosion can seriously reduce structural strength. FAA A&P corrosion control technicians must evaluate affected structure according to approved limits and repair data.
Filiform Corrosion
Filiform corrosion develops beneath protective coatings and appears as threadlike lines or small wormlike trails beneath paint.
It often begins where moisture enters through scratches, chips, improperly prepared surfaces, or broken coating edges.
Although filiform corrosion may initially appear cosmetic, the coating must be removed sufficiently to reveal the full extent of the attack before treatment.
Correct surface preparation and restoration of the protective finish help prevent recurrence.
Fretting Corrosion
Fretting corrosion occurs where tightly fitted surfaces experience small amounts of relative movement.
The movement wears away protective films and produces fine metal particles. Those particles oxidize and may appear as dark or reddish debris around joints, bearings, fittings, or riveted structures.
Fretting can indicate movement within a joint. A technician must address both the corrosion and the underlying mechanical condition that allowed the movement.
Stress-Corrosion Cracking

Stress-corrosion cracking results from the combined effects of sustained tensile stress and a corrosive environment.
The stress may come from:
- Applied loads
- Residual manufacturing stress
- Improper assembly
- Press fits
- Heat treatment
- Cold working
- Structural deformation
Stress-corrosion cracking is dangerous because cracks can develop with little visible surface corrosion. Highly stressed aircraft components require careful inspection and approved evaluation.
Removing visible corrosion does not automatically make a cracked or overstressed component serviceable.
Corrosion Fatigue
Corrosion fatigue occurs when cyclic loading and a corrosive environment act together.
Corrosion pits can become stress concentrations where fatigue cracks begin. As a result, a component may fail under lower cyclic loads than it would in a noncorrosive environment.
Prompt detection and treatment of corrosion are important because corrosion damage can affect both material thickness and fatigue resistance.
Corrosion-Prone Aircraft Areas
Corrosion can occur almost anywhere, but some aircraft locations deserve additional attention.
Exhaust-Trail Areas
Exhaust deposits may contain corrosive compounds. Areas behind engine exhaust outlets should be cleaned and inspected regularly.
Battery Compartments

Battery electrolyte and vapors can attack surrounding structure, wiring, fasteners, and equipment. Battery compartments, vents, drains, and adjacent areas require careful cleaning and inspection.
The neutralizing process depends on the battery chemistry and approved maintenance instructions. A chemical used for one battery type may be inappropriate for another.
Bilge and Lower-Fuselage Areas
Moisture, dirt, lavatory fluids, hydraulic fluid, and other contaminants can collect in low areas. Blocked drains increase the opportunity for corrosion.
Wheel Wells and Landing Gear
Wheel wells and landing gear are exposed to water, mud, runway chemicals, deicing materials, brake residue, and debris.
Engine Inlets and Cooling Openings
Engine frontal areas and cooling passages receive moisture, dirt, salt, and other airborne contaminants.
Lap Joints and Fasteners
Moisture can become trapped between overlapping sheets, around fasteners, beneath sealant, or under damaged paint.
Lavatories and Galleys

Spilled liquids, cleaning chemicals, food residue, and leaking plumbing can cause extensive hidden corrosion beneath flooring or interior panels.
Control-Surface and Hinge Areas
Hinges, bearings, and control-surface attachment points can trap moisture and may be exposed to dissimilar metals and mechanical movement.
Avionics Compartments and Mounting Racks
Moisture, dust, lint, cooling-air contamination, spilled fluids, and deteriorated seals can affect avionics racks, connectors, wiring, bonding straps, and electronic equipment.
Aircraft Washing and Exterior Cleaning

Aircraft washing removes dirt and contaminants before they damage finishes or conceal defects. This may be the first step in aircraft corrosion prevention.
Before washing an aircraft, technicians should:
- Review the manufacturer’s cleaning instructions
- Identify areas requiring protection
- Confirm that drain holes are open
- Protect pitot tubes, static ports, vents, and openings as required
- Protect windows and transparent plastics
- Use approved cleaning materials
- Follow environmental and wastewater requirements
- Prevent water from entering electrical or avionics equipment
Cleaning compounds must be correctly mixed and used at the approved concentration. A cleaner that is too strong can damage paint, sealant, plated surfaces, plastics, rubber, or metal.
High-pressure spray must not be directed into bearings, vents, static ports, electrical connectors, or other sensitive areas unless specifically permitted.
After washing, protective covers and tape must be removed and the aircraft inspected for trapped water or remaining contamination.
Cleaning Transparent Plastics
Aircraft windshields, windows, and other transparent plastics can be damaged by improper cleaners and wiping methods.
Dust and dirt should be removed using the aircraft manufacturer’s approved procedure. Dry wiping can scratch some transparent surfaces.
Technicians should avoid unapproved solvents, abrasive cleaners, dirty cloths, and materials that may create static electricity or surface damage.
Clean wiping material should be used, and the wiping direction should follow the manufacturer’s instructions. Damage such as crazing, clouding, scratches, delamination, or chemical attack must be evaluated properly.
Removing Oil and Grease
Oil and grease may require an approved solvent, emulsion cleaner, or other cleaning product.
The technician must consider:
- Surface material
- Protective coating
- Type of contamination
- Fire and ventilation hazards
- Compatibility with rubber, plastic, sealant, and wiring
- Required personal protective equipment
- Environmental restrictions
Unapproved solvents can soften paint, damage plastics, deteriorate insulation, or leave harmful residue.
Safety data sheets and the manufacturer’s maintenance information should be consulted before using chemical products.
Chemical Safety and Personal Protective Equipment

Aircraft cleaning and corrosion treatment can expose technicians to solvents, acids, alkaline compounds, paint removers, conversion coatings, dust, and metal particles.
Depending on the product and task, required protection may include:
- Chemical-resistant gloves
- Eye and face protection
- Protective clothing
- Respiratory protection
- Hearing protection
- Adequate ventilation
- Approved fire-protection equipment
Chemicals must be correctly labeled, stored, mixed, and disposed of. Technicians should never mix chemicals unless the approved procedure specifically requires it.
Environmental and hazardous-material requirements may vary by location and are subject to change.
Inspecting for Corrosion
Corrosion inspection begins with a clean surface and adequate access, lighting, and inspection equipment.
Warning signs include:
- Discoloration
- Powdery deposits
- Rust
- Paint blisters
- Flaking or lifting paint
- Surface roughness
- Pits
- Bulging around fasteners
- Distorted or lifted skin
- Cracks
- Swollen lap joints
- Loose fasteners
- Damaged sealant
- Corroded electrical connections
- Evidence of moisture entry
Paint and sealant may conceal corrosion. If approved instructions require coating removal, the technician must remove enough material to identify the full boundaries of the affected area.
After corrosion removal, the remaining material thickness and damage must be compared with approved limits.
Corrosion Severity and Repair Limits

Corrosion should not be classified only by appearance. Its location, depth, affected area, material, structural function, and effect on remaining strength must be evaluated.
Light surface corrosion may permit cleaning, treatment, and refinishing. More serious damage may require blending, additional inspection, part replacement, or an approved structural repair.
Technicians must not grind or blend away material without knowing the allowable limits. Excessive removal can weaken a component even when the surface appears smooth afterward.
The applicable Aircraft Maintenance Manual and manufacturer’s corrosion-control instructions should be consulted before treating or repairing damage.
Removing Corrosion
A typical corrosion-treatment process may include:
- Cleaning the affected area
- Removing paint or coatings as required
- Identifying the complete extent of corrosion
- Removing corrosion products by an approved method
- Inspecting for cracks or hidden damage
- Measuring remaining material when required
- Comparing the damage with allowable limits
- Applying the specified surface treatment
- Restoring primer, paint, sealant, or preservative
- Documenting the work as required
The correct removal method depends on the metal, component, location, and severity of the corrosion.
Abrasives approved for one metal may contaminate or damage another. For example, steel particles embedded in aluminum can create future corrosion problems.
Corrosion Treatment on Different Metals

Aluminum Alloys
Aluminum corrosion commonly produces a white or gray powder. Surface attack may progress into pitting, intergranular corrosion, or exfoliation.
Do not remove or damage the thin pure-aluminum surface layer on Alclad® material unnecessarily.
Magnesium Alloys
Magnesium is highly susceptible to corrosion and may show white, powdery, or bulky deposits. Protective coatings are particularly important.
Use only approved tools, materials, and treatment processes.
Ferrous Metals
Corrosion on ordinary steel generally appears as reddish-brown rust. Highly stressed steel parts require special care because aggressive corrosion removal can damage the surface or affect fatigue resistance.
Stainless Steel
Stainless steel relies on a passive oxide film for corrosion resistance. Contamination with ordinary steel particles can interfere with that protection and promote corrosion.
Titanium
Titanium has good corrosion resistance but can be damaged or contaminated by improper handling, chemicals, or high-temperature contact with certain materials.
Copper and Copper Alloys
Copper corrosion may appear as green, blue-green, black, or brown deposits. The location and approved condition of the component determine whether cleaning, treatment, or replacement is required.
Protective Coatings and Preservation
Once corrosion has been removed, the surface must be protected against renewed exposure.
Protection may include:
- Conversion coatings
- Primer and paint
- Sealants
- Plating
- Corrosion-preventive compounds
- Lubricants
- Moisture barriers
- Proper drainage
- Electrical bonding protection
Surface preparation is essential. Applying paint or preservative over contamination or remaining corrosion can conceal the problem without stopping it.
Technicians should inspect protective coatings regularly and promptly repair chips, scratches, cracks, or missing sealant.
Avionics Corrosion Under AC 43-206
AC 43-206 Change 1 applies specifically to systems and equipment that use or conduct electrical power. It covers avionics corrosion inspection, cleaning, preservation, treatment, electrical bonding, electromagnetic-interference protection, electrostatic-discharge-sensitive equipment, and emergency recovery.
Even a small amount of corrosion can create the following:

- Intermittent electrical faults
- Increased circuit resistance
- Poor bonding or grounding
- Connector failures
- Signal degradation
- Cooling problems
- Complete equipment failure
Avionics corrosion may affect the following:
- Electrical connectors
- Terminal strips
- Wiring
- Bonding straps
- Mounting racks
- Antennas and antenna bases
- Switches and relays
- Circuit boards
- Equipment housings
- EMI shielding
- Cooling-air passages
Students studying this area should also review Basic Electricity for FAA A&P Mechanics.
Cleaning Avionics and Electrical Equipment
Avionics cleaning requires special care because moisture, static electricity, cleaning residue, compressed air, brushes, or solvents can damage delicate components.
Before cleaning, technicians should:
- Remove electrical power
- Discharge and ground circuits as required
- Observe electrostatic-discharge precautions
- Identify the contamination
- Follow the equipment or aircraft manufacturer’s instructions
- Use only approved materials and equipment
- Protect connectors and components from additional contamination
- Dry the equipment using an approved process
AC 43-206 addresses mechanical cleaning, solvent cleaning, drying, preservation, packaging, handling, and storage. It supplements OEM recommendations or may provide guidance when OEM instructions are unavailable.
Electrical Bonding and Corrosion

Corrosion at an electrical bonding or grounding connection can increase resistance and interfere with the intended electrical path.
Poor bonding may affect:
- Lightning protection
- Static-electricity dissipation
- Radio performance
- Electromagnetic-interference control
- Fault-current paths
- System reliability
Bonding surfaces must be prepared, assembled, sealed, and tested according to approved procedures. Removing corrosion without correctly restoring the bonding connection can leave the aircraft with an electrical defect.
Emergency Avionics Cleaning
Fire-extinguishing agents, fresh water, saltwater, sewage, or other contaminants can rapidly damage avionics equipment.
Emergency action may involve:
- Removing electrical power
- Controlling safety hazards
- Establishing priorities
- Removing standing water and contaminants
- Beginning approved cleaning promptly
- Drying and preserving affected equipment
- Protecting electrostatic-discharge-sensitive components
- Sending equipment to an appropriately equipped repair facility
Saltwater exposure is particularly serious because salt deposits attract moisture and remain electrically conductive and corrosive.
Personnel should follow the manufacturer’s instructions and AC 43-206 rather than applying ordinary aircraft-washing methods to avionics equipment.
Corrosion Prevention and Control Programs

Effective aircraft corrosion control is a continuing cycle rather than a one-time repair.
A corrosion prevention and control program may include:
- Trained personnel
- Scheduled washing
- Regular inspections
- Cleaning exposed unpainted surfaces
- Keeping drains open
- Maintaining protective coatings
- Periodically renewing corrosion-preventive compounds
- Lubricating specified components
- Treating corrosion promptly
- Recording findings and repairs
- Adjusting inspection intervals for the operating environment
Early treatment generally reduces repair cost, aircraft downtime, and structural damage.
Corrosion control is an all-hands responsibility. Anyone who discovers coating damage, moisture entry, blocked drains, contamination, or corrosion should report it promptly.
Common FAA Test Mistakes
Students commonly miss cleaning and corrosion-control questions by:
- Confusing corrosion with erosion
- Forgetting one of the four elements of a corrosion cell
- Confusing galvanic and concentration-cell corrosion
- Misidentifying intergranular or exfoliation corrosion
- Assuming surface appearance reveals the full depth of damage
- Using the same cleaning material on every aircraft surface
- Selecting an incorrect neutralizing chemical
- Using steel tools or abrasives on aluminum
- Ignoring dissimilar-metal contact
- Treating corrosion without restoring the protective coating
- Assuming a small amount of avionics corrosion is harmless
- Using general guidance instead of manufacturer instructions
The best preparation is to understand how corrosion forms, how it appears, and why each cleaning or protective procedure is required.
How to Study Cleaning and Corrosion Control
Divide the subject into manageable areas:
- Purpose of aircraft cleaning
- Chemical and electrochemical corrosion
- The four elements of a corrosion cell
- Factors affecting corrosion
- Types of corrosion
- Corrosion-prone aircraft areas
- Exterior and interior cleaning
- Chemical and personal safety
- Corrosion inspection
- Corrosion removal and damage limits
- Treatment of different aircraft metals
- Protective coatings and preservation
- Avionics and electrical corrosion
- Corrosion prevention programs
Then reinforce the material with FAA General Knowledge practice quizzes.
When you miss a question, identify the form of corrosion, metal, environment, or maintenance principle involved. Read the explanation and use the applicable FAA reference to understand why the answer is correct.
Students can also review Aircraft Materials and Processes for FAA A&P Mechanics, Aircraft Ground Operations and Servicing, and How to Pass the FAA General Exam.
Prepare With Volarprep.com
Cleaning and corrosion control are important for passing the FAA General Knowledge test, but their value reaches far beyond the exam.
An A&P mechanic must recognize contamination, understand corrosion, protect aircraft materials, and know when damage requires further evaluation or approved repair data.
Volarprep.com helps future aviation maintenance technicians prepare with FAA-style practice questions and detailed explanations based on FAA handbooks, advisory circulars, certification standards, regulations, and extensive aircraft maintenance experience.
Explore FAA A&P study and practice-test options at Volarprep.com as you prepare for your General, Airframe, and Powerplant knowledge tests.
The free Volarprep.com reference pages help you understand and review the subject. Use them together with your FAA textbooks and handbooks for detailed study. Then use Volarprep.com FAA A&P practice tests to apply that knowledge to FAA-style questions, review answer explanations, and identify subjects that need more study.